Effect of dentin pretreatment with arginine on microshear bond strength of etch-and-rinse or self-etch adhesive systems
Gabriela Oliveira Borgo, Waldemir Francisco Vieira-Junior, Jéssica Dias Theobaldo, Flávio Henrique Baggio Aguiar, Débora Alves Nunes Leite Lima
ARTIGO
Inglês
Agradecimentos: This study was financed in part by the Coordenação de Aperfeiçoamento de Pessoal de Nível Superior - Brasil (CAPES) - Finance Code 001
Abstract: The main purpose of this study was to evaluate the effect of dentin pretreatment with 8% arginine on the immediate and 6-month bond strength (BS) of adhesive systems and surface morphology of dentin. Dentin bovine specimens (5 × 5 mm) were allocated into following pretreatments: without...
Ver mais
Abstract: The main purpose of this study was to evaluate the effect of dentin pretreatment with 8% arginine on the immediate and 6-month bond strength (BS) of adhesive systems and surface morphology of dentin. Dentin bovine specimens (5 × 5 mm) were allocated into following pretreatments: without pretreatment (conventional technique, C) or exposure to arginine solution (A) for 5 minutes prior to tooth restoration. The adhesive procedure was performed using (n = 12): 3-step etch-and-rinse adhesive (Scotchbond Multipurpose-SBMP [C+SBMP and A+SBMP]); 2-step etch-and-rinse adhesive (Single Bond 2 - SB [C+SB and A+SB]); or 2-step self-etch adhesive (Clearfil SE Bond - CSEB [C+CSEB and A+CSEB]). After 24 hours, the composite resin restorations were evaluated immediately and after 6 months of water storage using a microshear test and fracture pattern. The dentin surface exposed to A was assessed by scanning electron microscopy (SEM). The immediate BS data were submitted to a two-way analysis of variance and Tukey's test, and the long-term BS results were analyzed using Kruskal-Wallis and Dunn tests ('alpha' = 0.05). There was a significant decrease in immediate and 6-month BS for the A+SB and A+CSEB groups, which differed statistically from the C group. The fracture pattern was predominantly adhesive for SB and CSEB adhesive for C and A. The SEM images presented a different conditioning pattern of the dentin exposed to A. The dentin pretreatment with arginine interfered negatively in the immediate and long-term BS of the simplified adhesive system. However, the SBMP adhesive was not affected by arginine pretreatment presenting the most satisfactory results
Ver menos
COORDENAÇÃO DE APERFEIÇOAMENTO DE PESSOAL DE NÍVEL SUPERIOR - CAPES
001
Aberto
Effect of dentin pretreatment with arginine on microshear bond strength of etch-and-rinse or self-etch adhesive systems
Gabriela Oliveira Borgo, Waldemir Francisco Vieira-Junior, Jéssica Dias Theobaldo, Flávio Henrique Baggio Aguiar, Débora Alves Nunes Leite Lima
Effect of dentin pretreatment with arginine on microshear bond strength of etch-and-rinse or self-etch adhesive systems
Gabriela Oliveira Borgo, Waldemir Francisco Vieira-Junior, Jéssica Dias Theobaldo, Flávio Henrique Baggio Aguiar, Débora Alves Nunes Leite Lima
Fontes
European journal of dentistry (Fonte avulsa) |